申请号:EP82306792.1申请日:19821220公开号:EP0083190B1公开日:19860212

摘要:A polybutadiene rubber having an enhanced mechanical strength is produced insuch a manner that the contents of water and carbon disulfide in a solution of 1,3-butadiene and carbon disulfide in an inert organic solvent is controlled to 0.2 to 5 mmoles and 20 m moles or less, respectively, per liter of the 1,3-butadiene-carbondisulfide solution; a first polymerization mixture is prepared from the controlled 1,3-butadiene-carbon disulfide solution, an organic aluminum compound of the formula AlRX, wherein R = C alkyl, phenyl or cycloalkyl, X = halogen, and n = 1.5-2.0, and a cobaltcompound, for example, by aging a mixture of the controlled 1,3-butadiene-carbondisulfide solution with the aluminum compound for at least one minutes and then byadmixing the aged mixture with the cobalt compound; the first polymerization mixture issubjected to a cis-1,4- polymerization; a second polymerization comprising the resultantcis-1,4-polybutadiene, non-reacted 1,3-butadiene, the inert organic solvent, an organicaluminum compound of the formula AIR3, a cobalt compound, and the carbon disulfide issubjected to a 1,2-polymerization to produce a polybutadiene rubber consistingessentially of ε% to 30% by weight of a boiling n-hexane-insoluble fraction and 70% to

95% by weight of a boiling n-hexane-soluble fraction thereof; and after the 1,2-polymerization is shortstopped, the resultant polybutadiene rubber is isolated from the1,2- polymerization mixture.

申请人:UBE INDUSTRIES, LTD.